Customization: | Available |
---|---|
Grade Standard: | Industrial Grade |
Appearance: | Liquid |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Items | Standard | Result |
Ester content | 99.5min | 99.89 |
Color(pt-co rimetric) | 50max | 25 |
Destiny,(20ºC),g/cm3 | 0.984-0.991 | 0.988 |
Acidity | 0.10max | 0.085 |
Heat Loss (125ºC X 3 hrs) | 0.1max | 0.04 |
Refractive Index (nD 20ºC) | 1.485±0.003 | 1.486 |
Flash Point | 245max | 252 |
Moisture content % | 0.05max | 0.019 |
Volume Resistivity(Ω·cm)×1011 | 6.0min | 12.06 |
Totm mainly used for the raw materials of 105ºC grade heat resistant wire and cable as well as other products with higher heat resistance and durability requirements such as, plates, sheets, sealing pads and others. This product is also applicable to many kinds of plastic such as, cellulose nitrate, ethyl cellulose, and others.